Arkema Rilsan® AMN G8 TLD Nylon 12, Graphite Filled (Dry)


Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA12; Polyamide 12

Material Notes:
Designation ISO 1874-PA12,MHLS,14-010,CD05

Rigid grade with graphite filler for injection molding. Available colors: steel gray. Light and heat stabilized. Mold-release agent.

Low friction coefficient. No need of lubricant. Good mechanical properties. Easy filling of the mold due to its well adapted viscosity. Low shrinkage: include 1% on average for the design of the mold. Very good dimensional stability (low moisture absorption). Higher rate of production.

Example applications: Moving mechanical parts.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesMetricEnglishComments
Density1.02 g/cc0.0368 lb/in³ 
Water Absorption1.6 %1.6 % 
Melt Flow61.5 g/10 min61.5 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Yield45 MPa6530 psi 50 mm/min
Elongation at BreakMin 50 %Min 50 % Nominal Strain; 50 mm/min
Elongation at Yield10 %10 % 50 mm/min
Tensile Modulus1.52 GPa220 ksi 1 mm/min
Charpy Impact UnnotchedNBNB 
Charpy Impact, Notched, Low Temp0.4 J/cm²1.9 ft-lb/in² at -30°C
Charpy Impact, Unnotched Low TempNBNB 
Charpy Impact, Notched0.41 J/cm²1.95 ft-lb/in² 

Electrical Properties
Dissipation Factor0.0003320.000332 1 MHz
Dissipation Factor, Low Frequency0.000450.00045 100 Hz

Thermal Properties
Melting Point174 °C345 °F 10°C/min
Flammability, UL94HBHB 3.1 mm
Flammability, UL94HBHB 1.6 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.