Arkema Rilsan® AMN P30 LD Nylon 12, Flexible, Injection Grade (Conditioned)


Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA12; Polyamide 12

Material Notes:
Designation ISO 1874-PA12-P,MLR,12-004

Flexible grade for injection molding. Available color: black. Light stabilized. Mold-release agent.

Good impact strength. Flexibility and dynamic properties. Easy filling of the mold due to its well adapted viscosity. Low shrinkage: include 1% on average for the design of the mold. Good dimensional stability (low moisture absorption).

UL classification: UL94 HB RTI(C) 65/65/65.

Example applications: Cable ties and clips.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesMetricEnglishComments
Density1.03 g/cc0.0372 lb/in³ 
Melt Flow61.3 g/10 min61.3 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Yield28 MPa4060 psi 50 mm/min
Elongation at BreakMin 50 %Min 50 % Nominal Strain; 50 mm/min
Elongation at Yield22 %22 % 50 mm/min
Tensile Modulus0.545 GPa79 ksi 1 mm/min
Charpy Impact UnnotchedNBNB 
Charpy Impact, Notched, Low Temp0.37 J/cm²1.76 ft-lb/in² at -30°C
Charpy Impact, Unnotched Low TempNBNB 
Charpy Impact, Notched2.17 J/cm²10.3 ft-lb/in² 

Electrical Properties
Electrical Resistivity1e+011 ohm-cm1e+011 ohm-cm 
Surface Resistance5e+011 ohm5e+011 ohm 
Dielectric Strength25 kV/mm635 kV/in 
Comparative Tracking Index600 V600 V 

Thermal Properties
CTE, linear 20°C140 µm/m-°C77.8 µin/in-°F Parallel to flow
Melting Point168 °C334 °F (Dry)
Deflection Temperature at 0.46 MPa (66 psi)125 °C257 °F 
Deflection Temperature at 1.8 MPa (264 psi)47 °C117 °F 
Vicat Softening Point133 °C271 °F 50°C/hr; 50N
Flammability, UL94HBHB 3.1 mm
Flammability, UL94HBHB 1.6 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.