Arkema Rilsan® AMN Y TLD Nylon 12, MoS2 Filled (Conditioned)


Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA12; Polyamide 12

Material Notes:
Designation ISO 1874-PA12,MHLS,14-010,MD05

Grade with molybdenum filler for injection molding. Available color: steel gray. Light and heat stabilized. Mold-release agent.

Low friction coefficient. Good impact strength. Easy filling of the mold due to its well adapted viscosity. Low shrinkage: include 1% on average for the design of the mold. Very good dimensional stability (low moisture absorption).

Example applications: Moving mechanical parts such as gear.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesOriginal ValueComments
Density1.02 g/cc 
Melt Flow50 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Yield39 MPa 50 mm/min
Elongation at BreakMin 50 % Nominal Strain; 50 mm/min
Elongation at Yield12 % 50 mm/min
Tensile Modulus1.38 GPa 1 mm/min

Electrical Properties
Electrical Resistivity1e+014 ohm-cm 
Surface Resistance1e+014 ohm 
Dielectric Strength55 kV/mm 
Comparative Tracking Index600 V 

Thermal Properties
CTE, linear 20°C90 µm/m-°C Parallel to flow
Melting Point174 °C (Dry)
Deflection Temperature at 0.46 MPa (66 psi)143 °C 
Deflection Temperature at 1.8 MPa (264 psi)65 °C 
Vicat Softening Point145 °C 50°C/hr; 50N
Flammability, UL94HB 1.6 mm
Flammability, UL94V-2 3.2 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.