MatWeb, The Online Materials Database

Arkema Rilsan® AMV TL Nylon 12, Rigid, Injection Grade (Conditioned)


Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA12; Polyamide 12

Material Notes:
Designation ISO 1874-PA12,MHLR,16-010

Rigid grade for injection molding. Available color: natural. Light and heat stabilized. Mold-release agent.

High impact strength. Easy filling of the mold due to its well adapted viscosity. Low shrinkage: include 1% on average for the design of the mold. Very good dimensional stability (low moisture absorption).

Example applications: Parts for all technology with high impact strength requirements.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesMetricEnglishComments
Density1.01 g/cc0.0365 lb/in³ 
Melt Flow5.3 g/10 min5.3 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Yield38 MPa5510 psi 50 mm/min
Elongation at BreakMin 50 %Min 50 % Nominal Strain; 50 mm/min
Elongation at Yield12 %12 % 50 mm/min
Tensile Modulus1.02 GPa148 ksi 1 mm/min
Charpy Impact UnnotchedNBNB 
Charpy Impact, Notched, Low Temp0.58 J/cm²2.76 ft-lb/in² at -30°C
Charpy Impact, Unnotched Low TempNBNB 
Charpy Impact, Notched0.69 J/cm²3.28 ft-lb/in² 

Electrical Properties
Electrical Resistivity1e+014 ohm-cm1e+014 ohm-cm 
Surface Resistance1e+014 ohm1e+014 ohm 
Dielectric Strength30 kV/mm762 kV/in 
Comparative Tracking Index600 V600 V 

Thermal Properties
CTE, linear 20°C100 µm/m-°C55.6 µin/in-°F Parallel to flow
Melting Point174 °C345 °F (Dry)
Deflection Temperature at 0.46 MPa (66 psi)135 °C275 °F 
Deflection Temperature at 1.8 MPa (264 psi)55 °C131 °F 
Vicat Softening Point142 °C288 °F 50°C/hr; 50N
Flammability, UL94HBHB 1.6 mm
Flammability, UL94V-2V-2 3.2 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.