Arkema Rilsan® ARVO 950 TLD Nylon 12, Rotomolding Grade (Conditioned)


Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA12; Polyamide 12

Material Notes:
Designation ISO 1874-PA12,RHLR,16-010

Grade for rotomolding. Available color: natural. Light and heat stabilized. Mold-release agent.

Easy to be processed in the same conditions as polyethylene. High thermal and chemical resistance. Outstanding mechanical properties. Low permeability to gas and hydrocarbon.

Example applications: Oil tank, hydraulic fluid tank.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesMetricEnglishComments
Density1.01 g/cc0.0365 lb/in³ 

Mechanical Properties
Tensile Strength, Yield40 MPa5800 psi 50 mm/min
Elongation at BreakMin 50 %Min 50 % Nominal Strain; 50 mm/min
Elongation at Yield11 %11 % 50 mm/min
Tensile Modulus1.08 GPa157 ksi 1 mm/min
Charpy Impact UnnotchedNBNB 
Charpy Impact, Notched, Low Temp0.59 J/cm²2.81 ft-lb/in² at -30°C
Charpy Impact, Unnotched Low TempNBNB 
Charpy Impact, Notched0.67 J/cm²3.19 ft-lb/in² 

Electrical Properties
Electrical Resistivity1e+014 ohm-cm1e+014 ohm-cm 
Surface Resistance1e+014 ohm1e+014 ohm 
Dielectric Strength30 kV/mm762 kV/in 
Comparative Tracking Index600 V600 V 

Thermal Properties
CTE, linear 20°C100 µm/m-°C55.6 µin/in-°F Parallel to flow
Deflection Temperature at 0.46 MPa (66 psi)135 °C275 °F 
Deflection Temperature at 1.8 MPa (264 psi)55 °C131 °F 
Vicat Softening Point142 °C288 °F 50°C/hr; 50N

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.