MatWeb, The Online Materials DatabaseArkema RilsanŽ ASR 20 Nylon 12, 20% Carbon Fiber Filled (Dry)Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic Close Analogs: Key Words: PA12; Polyamide 12 Material Notes: Rigid grade with carbon fiber filler (20%) for injection molding. Available color: black. High strength-to-weight ratio. Very low shrinkage: include 0,5% on average for the design of the mold. High dimensional stability (low moisture absorption). Antistatic properties. Example applications: Parts with high mechanical properties and dimensional precision. ISO data provided by the manufacturer, Arkema.
|
|||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Copyright 1996-2010 by Automation Creations, Inc. The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb. |