Designation ISO 1874-PA12,M,16-090,CF20

Rigid grade with carbon fiber filler (20%) for injection molding. Available color: black. High strength-to-weight ratio. Very low shrinkage: include 0,5% on average for the design of the mold. High dimensional stability (low moisture absorption). Antistatic properties.

Example applications: Parts with high mechanical properties and dimensional precision.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesMetricEnglishComments
Density1.1 g/cc0.0397 lb/in³ 
Melt Flow4.6 g/10 min4.6 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Ultimate128 MPa18600 psi 5 mm/min
Elongation at Break4 %4 % 5 mm/min
Tensile Modulus11.4 GPa1650 ksi 1 mm/min
Charpy Impact Unnotched6.37 J/cm²30.3 ft-lb/in² 
Charpy Impact, Notched, Low Temp1 J/cm²4.76 ft-lb/in² at -30°C
Charpy Impact, Unnotched Low Temp5.83 J/cm²27.7 ft-lb/in² at -30°C
Charpy Impact, Notched1.73 J/cm²8.23 ft-lb/in² 

Electrical Properties
Electrical Resistivity600 ohm-cm600 ohm-cm 
Dielectric Strength1 kV/mm25.4 kV/in 
Comparative Tracking Index100 V100 V 

Thermal Properties
CTE, linear 20°C40 µm/m-°C22.2 µin/in-°F Parallel to flow
Melting Point174 °C345 °F (Dry)
Deflection Temperature at 0.46 MPa (66 psi)175 °C347 °F 
Deflection Temperature at 1.8 MPa (264 psi)160 °C320 °F 
Vicat Softening Point170 °C338 °F 50°C/hr; 50N
Flammability, UL94HBHB 3.1 mm
Flammability, UL94HBHB 1.6 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.