MatWeb, The Online Materials DatabaseArkema Rilsan® AUM 30 T6LD Nylon 12, 30% Glass Bead Filled (Dry)Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic Close Analogs: Key Words: PA12; Polyamide 12 Material Notes: Rigid grad with glass beads filler (30%) for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent. Reinforced isotropic performances. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. High dimensional stability (low moisture absorption). Low coefficient of linear expansion. Example applications: Mechanical parts with dimensional precision. ISO data provided by the manufacturer, Arkema.
|
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Copyright 1996-2010 by Automation Creations, Inc. The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb. |