MatWeb, The Online Materials Database

Arkema Rilsan® AUM 30 T6LD Nylon 12, 30% Glass Bead Filled (Conditioned)


Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA12; Polyamide 12

Material Notes:
Designation ISO 1874-PA12,MHLR,16-020,GB30

Rigid grad with glass beads filler (30%) for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.

Reinforced isotropic performances. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. High dimensional stability (low moisture absorption). Low coefficient of linear expansion.

Example applications: Mechanical parts with dimensional precision.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesOriginal ValueComments
Density1.22 g/cc 
Melt Flow70.8 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Yield39 MPa 50 mm/min
Elongation at Break32 % Nominal Strain; 50 mm/min
Elongation at Yield6 % 50 mm/min
Tensile Modulus1.72 GPa 1 mm/min
Charpy Impact Unnotched4.72 J/cm² 
Charpy Impact, Notched, Low Temp0.45 J/cm² at -30°C
Charpy Impact, Unnotched Low Temp4.95 J/cm² at -30°C
Charpy Impact, Notched0.56 J/cm² 

Electrical Properties
Electrical Resistivity1e+013 ohm-cm 
Surface Resistance1e+013 ohm 
Dielectric Strength40 kV/mm 
Comparative Tracking Index600 V 

Thermal Properties
CTE, linear 20°C70 µm/m-°C Parallel to flow
Melting Point174 °C (Dry)
Deflection Temperature at 0.46 MPa (66 psi)155 °C 
Deflection Temperature at 1.8 MPa (264 psi)60 °C 
Vicat Softening Point160 °C 50°C/hr; 50N
Flammability, UL94HB 3.1 mm
Flammability, UL94HB 1.6 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.