MatWeb, The Online Materials Database

Arkema Rilsan® AUM 50 NOIR T6LD Nylon 12, 50% Glass Bead Filled (Dry)


Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA12; Polyamide 12

Material Notes:
Designation ISO 1874-PA12,MHLR,16-020,GB50

Rigid grad with glass beads filler (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agents. Mold-release agent.

Good mechanical properties. Reinforced isotropic performances. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. High dimensional stability (low moisture absorption). Low coefficient of linear expansion.

Potable water contact approval WRC 950 1509.

Example applications: Mechanical parts with dimensional precision.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesMetricEnglishComments
Density1.42 g/cc0.0513 lb/in³ 
Water Absorption1 %1 % 
Melt Flow5 g/10 min5 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Yield52 MPa7540 psi 50 mm/min
Elongation at Break18 %18 % Nominal Strain; 50 mm/min
Elongation at Yield4 %4 % 50 mm/min
Tensile Modulus3.64 GPa528 ksi 1 mm/min
Charpy Impact Unnotched8.11 J/cm²38.6 ft-lb/in² 
Charpy Impact, Notched, Low Temp0.35 J/cm²1.67 ft-lb/in² at -30°C
Charpy Impact, Unnotched Low Temp7.6 J/cm²36.2 ft-lb/in² at -30°C
Charpy Impact, Notched0.42 J/cm²2 ft-lb/in² 

Electrical Properties
Dissipation Factor0.0004230.000423 1 MHz
Dissipation Factor, Low Frequency0.000530.00053 100 Hz

Thermal Properties
Melting Point174 °C345 °F 10°C/min
Flammability, UL94HBHB 3.1 mm
Flammability, UL94HBHB 1.6 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.