MatWeb, The Online Materials DatabaseArkema RilsanŽ AUM 50 NOIR T6LD Nylon 12, 50% Glass Bead Filled (Dry)Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic Close Analogs: Key Words: PA12; Polyamide 12 Material Notes: Rigid grad with glass beads filler (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agents. Mold-release agent. Good mechanical properties. Reinforced isotropic performances. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. High dimensional stability (low moisture absorption). Low coefficient of linear expansion. Potable water contact approval WRC 950 1509. Example applications: Mechanical parts with dimensional precision. ISO data provided by the manufacturer, Arkema.
|
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Copyright 1996-2010 by Automation Creations, Inc. The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb. |