Arkema RilsanŽ AZM 15 TLD Nylon 12, 15% Glass Fiber Filled (Conditioned)


Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA12; Polyamide 12

Material Notes:
Designation ISO 1874-PA12,MHLR,16-030,GF15

Rigid grade with glass fiber filler (15%) for injection molding.

Available color: natural. Light and heat stabilized. Mold-release agent.

Rigidity combined with good impact strength. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. Low coefficient of linear expansion. High dimensional stability.

Example applications: Mechanical fittings.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesOriginal ValueComments
Melt Flow12.9 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Ultimate72 MPa 5 mm/min
Elongation at Break8 % 5 mm/min
Tensile Modulus3.83 GPa 1 mm/min
Charpy Impact Unnotched6.4 J/cm˛ 
Charpy Impact, Notched, Low Temp0.72 J/cm˛ at -30°C
Charpy Impact, Unnotched Low Temp6.87 J/cm˛ at -30°C
Charpy Impact, Notched1.15 J/cm˛ 

Thermal Properties
Vicat Softening Point151 °C 50°C/hr; 50N

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.