MatWeb, The Online Materials DatabaseArkema Rilsan® AZM 23 G9 T6LD Nylon 12, 23% Glass Fiber Filled (Dry)Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic Close Analogs: Key Words: PA12; Polyamide 12 Material Notes: Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stabilizing agent. Mold-release agent. Rigidity. Low friction coefficient. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. Low coefficient of linear expansion. High dimensional stability. Example applications: Mechanical parts with friction such as gear and bearing. ISO data provided by the manufacturer, Arkema.
|
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Copyright 1996-2010 by Automation Creations, Inc. The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb. |