Arkema Rilsan® AZM 23 G9 T6LD Nylon 12, 23% Glass Fiber Filled (Conditioned)


Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA12; Polyamide 12

Material Notes:
Designation ISO 1874-PA12,MHLR,16-050,(G+C)(F+D)(23+05)

Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stabilizing agent. Mold-release agent.

Rigidity. Low friction coefficient. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. Low coefficient of linear expansion. High dimensional stability.

Example applications: Mechanical parts with friction such as gear and bearing.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesOriginal ValueComments
Density1.2 g/cc 
Melt Flow3.7 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Ultimate99 MPa 5 mm/min
Elongation at Break4 % 5 mm/min
Tensile Modulus6.6 GPa 1 mm/min
Charpy Impact Unnotched7.03 J/cm² 
Charpy Impact, Notched, Low Temp0.96 J/cm² at -30°C
Charpy Impact, Unnotched Low Temp7.28 J/cm² at -30°C
Charpy Impact, Notched1.23 J/cm² 

Electrical Properties
Electrical Resistivity1e+012 ohm-cm 
Surface Resistance1e+011 ohm 
Dielectric Strength20 kV/mm 
Comparative Tracking Index300 V 

Thermal Properties
CTE, linear 20°C60 µm/m-°C Parallel to flow
Melting Point174 °C (Dry)
Deflection Temperature at 0.46 MPa (66 psi)173 °C 
Deflection Temperature at 1.8 MPa (264 psi)165 °C 
Vicat Softening Point165 °C 50°C/hr; 50N
Flammability, UL94HB 3.1 mm
Flammability, UL94HB 1.6 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.