Arkema Rilsan® AZM 23 T6LD Nylon 12, 23% Glass Fiber Filled (Dry)


Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA12; Polyamide 12

Material Notes:
Designation ISO 1874-PA12,MHLR,16-050,GF23

Rigid grade with glass fiber filler (23%) for injection molding. Available colors: black and natural. Reinforced light and heat stabilizing agent. Mold-release agent.

Rigidity. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. Low coefficient of linear expansion. High dimensional stability.

Example applications: Rigid mechanical parts.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesOriginal ValueComments
Melt Flow3.2 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Ultimate85 MPa 5 mm/min
Elongation at Break6 % 5 mm/min
Tensile Modulus5.48 GPa 1 mm/min

Electrical Properties
Dissipation Factor0.000357 1 MHz
Dissipation Factor, Low Frequency0.000522 100 Hz

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.