Arkema Rilsan® AZM 30 NOIR T6LD Nylon 12, 30% Glass Fiber Filled (Dry)


Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA12; Polyamide 12

Material Notes:
Designation ISO 1874-PA12,MHLR,16-060,GF30

Rigid grade with glass fiber (30%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.

High rigidity. High compressive strength. Good thermal properties. Very low shrinkage: include 0,5% on average for the design of the mold. Low coefficient of linear expansion. High dimensional stability.

UL classification: UL94 HB (3,05mm) RTI(C) 110/105/110

Example applications: Quick connectors.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesMetricEnglishComments
Density1.24 g/cc0.0448 lb/in³ 
Water Absorption1.2 %1.2 % 
Melt Flow4.8 g/10 min4.8 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Ultimate112 MPa16200 psi 5 mm/min
Elongation at Break5 %5 % 5 mm/min
Tensile Modulus8 GPa1160 ksi 1 mm/min

Electrical Properties
Dielectric Strength35.5 kV/mm902 kV/in 
Dissipation Factor0.0003450.000345 1 MHz
Dissipation Factor, Low Frequency0.00040.0004 100 Hz
Comparative Tracking Index600 V600 V 

Thermal Properties
Melting Point174 °C345 °F 10°C/min
Flammability, UL94HBHB 3.1 mm
Flammability, UL94HBHB 1.6 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.