Material Notes:
Designation ISO 1874-PA12,MHLR,16-060,GF30

Rigid grade with glass fiber (30%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.

High rigidity. High compressive strength. Good thermal properties. Very low shrinkage: include 0,5% on average for the design of the mold. Low coefficient of linear expansion. High dimensional stability.

UL classification: UL94 HB (3,05mm) RTI(C) 110/105/110

Example applications: Quick connectors.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesOriginal ValueComments
Density1.24 g/cc 
Melt Flow4.8 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Ultimate108 MPa 5 mm/min
Elongation at Break5 % 5 mm/min
Tensile Modulus7.43 GPa 1 mm/min
Charpy Impact Unnotched7.7 J/cm² 
Charpy Impact, Notched, Low Temp0.98 J/cm² at -30°C
Charpy Impact, Unnotched Low Temp6.39 J/cm² at -30°C
Charpy Impact, Notched1.63 J/cm² 

Electrical Properties
Electrical Resistivity1e+013 ohm-cm 
Surface Resistance1e+014 ohm 
Dielectric Strength45 kV/mm 
Comparative Tracking Index600 V 

Thermal Properties
CTE, linear 20°C50 µm/m-°C Parallel to flow
Melting Point174 °C (Dry)
Deflection Temperature at 0.46 MPa (66 psi)175 °C 
Deflection Temperature at 1.8 MPa (264 psi)170 °C 
Vicat Softening Point165 °C 50°C/hr; 50N
Flammability, UL94HB 3.1 mm
Flammability, UL94HB 1.6 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.