MatWeb, The Online Materials Database

Arkema Rilsan® AZM 30 O TLD Nylon 12, 30% Glass Fiber Filled (Dry)


Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA12; Polyamide 12

Material Notes:
Designation ISO 1874-PA12,MHLR,16-050,GF30

Rigid grade with glass fiber (30%) for injection molding. Available color: natural. Light and heat stabilizing agent. Mold-release agent.

High rigidity. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. Low coefficient of linear expansion. High dimensional stability.

UL classification: UL94 HB (3,05mm) RTI(C) 65/65/65

Example applications: Mechanical parts with high rigidity.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesMetricEnglishComments
Density1.24 g/cc0.0448 lb/in³ 
Water Absorption1.2 %1.2 % 
Melt Flow6.7 g/10 min6.7 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Ultimate121 MPa17500 psi 5 mm/min
Elongation at Break5 %5 % 5 mm/min
Tensile Modulus8.82 GPa1280 ksi 1 mm/min

Electrical Properties
Dissipation Factor0.000360.00036 1 MHz
Dissipation Factor, Low Frequency0.000440.00044 100 Hz

Thermal Properties
Melting Point174 °C345 °F 10°C/min
Flammability, UL94HBHB 3.1 mm
Flammability, UL94HBHB 1.6 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.