MatWeb, The Online Materials Database

Arkema Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Dry)


Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA12; Polyamide 12

Material Notes:
Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05)

Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stabilizing agent. Mold-release agent.

High rigidity. Low friction coefficient. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. Low coefficient of linear expansion. High dimensional stability.

Example applications: Mechanical parts with friction such as gear and bearing.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesMetricEnglishComments
Density1.39 g/cc0.0502 lb/in³ 
Water Absorption1 %1 % 
Melt Flow2.3 g/10 min2.3 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Ultimate138 MPa20000 psi 5 mm/min
Elongation at Break4 %4 % 5 mm/min
Tensile Modulus13.3 GPa1930 ksi 1 mm/min
Charpy Impact Unnotched6.87 J/cm²32.7 ft-lb/in² 
Charpy Impact, Notched, Low Temp1.06 J/cm²5.04 ft-lb/in² at -30°C
Charpy Impact, Unnotched Low Temp6.87 J/cm²32.7 ft-lb/in² at -30°C
Charpy Impact, Notched1.26 J/cm²6 ft-lb/in² 

Thermal Properties
Melting Point174 °C345 °F 10°C/min
Flammability, UL94HBHB 3.1 mm
Flammability, UL94HBHB 1.6 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.