Designation ISO 1874-PA12,MHLR,16-090,GF50

Rigid grade with glass fiber (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.

High rigidity. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. Low coefficient of linear expansion. High dimensional stability.

Example applications: Mechanical parts with very high rigidity.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesMetricEnglishComments
Density1.41 g/cc0.0509 lb/in³ 
Melt Flow1.1 g/10 min1.1 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Ultimate145 MPa21000 psi 5 mm/min
Elongation at Break4 %4 % 5 mm/min
Tensile Modulus14.8 GPa2150 ksi 1 mm/min
Charpy Impact Unnotched8.58 J/cm²40.8 ft-lb/in² 
Charpy Impact, Notched, Low Temp1.72 J/cm²8.19 ft-lb/in² at -30°C
Charpy Impact, Unnotched Low Temp9.29 J/cm²44.2 ft-lb/in² at -30°C
Charpy Impact, Notched2.29 J/cm²10.9 ft-lb/in² 

Electrical Properties
Electrical Resistivity1e+012 ohm-cm1e+012 ohm-cm 
Surface Resistance1e+011 ohm1e+011 ohm 

Thermal Properties
CTE, linear 20°C30 µm/m-°C16.7 µin/in-°F Parallel to flow
Deflection Temperature at 0.46 MPa (66 psi)175 °C347 °F 
Deflection Temperature at 1.8 MPa (264 psi)170 °C338 °F 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.