MatWeb, The Online Materials Database

Arkema RilsanŽ MA 4420 Nylon 12, Flexible Tubing Grade (Dry)


Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PA11; Polyamide 11

Material Notes:
Designation ISO 1874-PA12-HI,EHL,22-003

Flexible grade for tubes extrusion. Available color: black. Light and heat stabilized.

Flexibility. High burst pressure and impact strength. Fit for use in a wide range of temperature. Very good chemical resistance.

Example applications: Tubes for air brake system in trucks approved by ISO 7628, DIN 73378 (PA12-PHLY), NFR 12632, SAEJ 844.

ISO data provided by the manufacturer, Arkema.

Physical PropertiesOriginal ValueComments
Water Absorption1.2 % 
Moisture Absorption at Equilibrium0.55 % Humidity Absorption
Melt Flow4.8 g/10 min 235°C/2.16 kg load

Mechanical Properties
Tensile Strength, Yield33 MPa 50 mm/min
Elongation at BreakMin 50 % Nominal Strain; 50 mm/min
Elongation at Yield19 % 50 mm/min
Tensile Modulus0.72 GPa 1 mm/min
Charpy Impact UnnotchedNB 
Charpy Impact, Notched, Low Temp0.43 J/cm˛ at -30°C
Charpy Impact, Unnotched Low TempNB 
Charpy Impact, Notched1.6 J/cm˛ 

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)42 °C 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.