MatWeb, The Online Materials Database

Bayer MaterialScience Texin® 185 Urethane Thermoplastic Elastomer


Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic

Key Words: TPU

Material Notes:
Key Features:

  • Unfilled

Suitable processing methods:

  • Injection molding
  • Film extrusion
  • Profile extrusion
  • Sheet extrusion
  • Coating

Information provided by Bayer Polymers.

Physical PropertiesMetricEnglishComments
Density1.26 g/cc0.0455 lb/in³ 

Mechanical Properties
Tensile Strength, Yield6 MPa870 psi Stress at 50% Strain
Elongation at BreakMin 50 %Min 50 % 

Thermal Properties
Vicat Softening Point88 °C190 °F 50°C/h 50N
Glass Temperature-30 °C-22 °F 10°C/min

Processing Properties
Melt Temperature195 °C383 °F Injection Molding
Mold Temperature30 °C86 °F Injection Molding
Injection Pressure45 MPa6530 psi 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.