MatWeb, The Online Materials Database

Bayer MaterialScience Texin® 245 Urethane Thermoplastic Elastomer


Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic

Key Words: TPU

Material Notes:
Key Features:

  • Unfilled

Suitable processing methods:

  • Injection molding

Information provided by Bayer Polymers.

Physical PropertiesOriginal ValueComments
Density1.21 g/cc 

Mechanical Properties
Tensile Strength, Yield8 MPa Stress at 50% Strain
Elongation at BreakMin 50 % 

Thermal Properties
Vicat Softening Point148 °C 50°C/h 50N
Glass Temperature-46 °C 10°C/min
Flammability, UL94HB 1.5 mm UL Recognized

Processing Properties
Melt Temperature205 °C Injection Molding
Mold Temperature30 °C Injection Molding
Injection Pressure45 MPa 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.