Bayer MaterialScience Texin® 950 Urethane Thermoplastic Elastomer


Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic

Key Words: TPU

Material Notes:
Key Features:

  • Unfilled

Suitable processing methods:

  • Injection molding
  • Profile extrusion
  • Sheet extrusion

Information provided by Bayer Polymers.

Physical PropertiesOriginal ValueComments
Density1.15 g/cc 

Mechanical Properties
Tensile Strength, Yield8 MPa Stress at 50% Strain
Elongation at BreakMin 50 % 

Electrical Properties
Volume Resistivity5e+010 ohm-cm 
Surface Resistance1e+012 ohm 
Dielectric Constant5.1 1 MHz
Dielectric Constant6.6 100 Hz
Dielectric Strength14.8 kV/mm 
Dissipation Factor0.025 100 Hz
Dissipation Factor0.075 1 MHz

Thermal Properties
CTE, linear 20°C224 µm/m-°C Parallel
Vicat Softening Point128 °C 50°C/h 50N
Glass Temperature-27 °C 10°C/min

Processing Properties
Melt Temperature205 °C Injection Molding
Mold Temperature30 °C Injection Molding
Injection Pressure45 MPa 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.