MatWeb, The Online Materials Database

Bayer MaterialScience Texin® 950U Urethane Thermoplastic Elastomer


Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic

Key Words: TPU

Material Notes:
Key Features:

  • Unfilled
  • U.V. stabilized or stable to weather

Suitable processing methods:

  • Injection molding
  • Profile extrusion
  • Sheet extrusion

Information provided by Bayer Polymers.

Physical PropertiesMetricEnglishComments
Density1.15 g/cc0.0415 lb/in³ 

Thermal Properties
CTE, linear 20°C103 µm/m-°C57.2 µin/in-°F Parallel
Vicat Softening Point128 °C262 °F 50°C/h 50N
Glass Temperature-27 °C-16.6 °F 10°C/min

Processing Properties
Melt Temperature205 °C401 °F Injection Molding
Mold Temperature35 °C95 °F Injection Molding
Injection Pressure45 MPa6530 psi 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.