Bayer MaterialScience Texin® 990R Urethane Thermoplastic Elastomer


Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic

Key Words: TPU

Material Notes:
Key Features:

  • Unfilled

Suitable processing methods:

  • Injection molding
  • Film extrusion
  • Profile extrusion
  • Sheet extrusion
  • Coating
  • Blow molding

Information provided by Bayer Polymers.

Physical PropertiesMetricEnglishComments
Density1.13 g/cc0.0408 lb/in³ 

Mechanical Properties
Tensile Strength, Yield5 MPa725 psi Stress at 50% Strain
Elongation at BreakMin 50 %Min 50 % 

Thermal Properties
Vicat Softening Point106 °C223 °F 50°C/h 50N
Glass Temperature-44 °C-47.2 °F 10°C/min

Processing Properties
Melt Temperature200 °C392 °F Injection Molding
Mold Temperature35 °C95 °F Injection Molding
Injection Pressure45 MPa6530 psi 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.