MatWeb, The Online Materials Database

Bayer MaterialScience Texin® 4210 Urethane Thermoplastic Elastomer


Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic

Key Words: TPU

Material Notes:
Key Features:

  • Unfilled

Suitable processing methods:

  • Injection molding
  • Film extrusion
  • Profile extrusion
  • Sheet extrusion

Information provided by Bayer Polymers.

Physical PropertiesMetricEnglishComments
Density1.21 g/cc0.0437 lb/in³ 

Mechanical Properties
Tensile Strength, Yield12 MPa1740 psi Stress at 50% Strain
Elongation at BreakMin 50 %Min 50 % 

Thermal Properties
CTE, linear 20°C131 µm/m-°C72.8 µin/in-°F Parallel
Deflection Temperature at 0.46 MPa (66 psi)98 °C208 °F 
Deflection Temperature at 1.8 MPa (264 psi)59 °C138 °F 
Vicat Softening Point139 °C282 °F 50°C/h 50N
Glass Temperature-35 °C-31 °F 10°C/min

Processing Properties
Melt Temperature230 °C446 °F Injection Molding
Mold Temperature30 °C86 °F Injection Molding
Injection Pressure45 MPa6530 psi 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.