Physical PropertiesOriginal ValueComments
Density1.2 g/cc 

Mechanical Properties
Tensile Strength, Yield7 MPa Stress at 50% Strain
Elongation at BreakMin 50 % 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.