DSM Engineering Plastics Stanyl® 46HF4130 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, High Flow (North America)


Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 46; Polymer; Thermoplastic

Key Words: Polyamide 46

Material Notes:
Information provided by DSM Engineering Plastics.

Physical PropertiesMetricEnglishComments
Density1.41 g/cc0.0509 lb/in³ (DAM); ISO 1183

Mechanical Properties
Tensile Strength at Break115 MPa16700 psi ISO 527-1/-2
Elongation at Break6 %6 % ISO 527-1/-2
Tensile Modulus6 GPa870 ksi ISO 527-1/-2
Charpy Impact Unnotched9 J/cm²42.8 ft-lb/in² ISO 179/1eU
Charpy Impact, Notched, Low Temp1.7 J/cm²8.09 ft-lb/in² at -30°C; ISO 179/1eU
Charpy Impact, Unnotched Low Temp6 J/cm²28.6 ft-lb/in² at -30°C; ISO 179/1eU
Charpy Impact, Notched1.7 J/cm²8.09 ft-lb/in² ISO 179/1eU

Thermal Properties
Melting Point295 °C563 °F (DAM); ISO 11357-1/-3

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.