DSM Engineering Plastics Stanyl® 46HF4130 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, High Flow (North America)


Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 46; Polymer; Thermoplastic

Key Words: Polyamide 46

Material Notes:
Information provided by DSM Engineering Plastics.

Physical PropertiesOriginal ValueComments
Density1.41 g/cc (DAM); ISO 1183

Mechanical Properties
Tensile Strength at Break115 MPa ISO 527-1/-2
Elongation at Break6 % ISO 527-1/-2
Tensile Modulus6 GPa ISO 527-1/-2
Charpy Impact Unnotched9 J/cm² ISO 179/1eU
Charpy Impact, Notched, Low Temp1.7 J/cm² at -30°C; ISO 179/1eU
Charpy Impact, Unnotched Low Temp6 J/cm² at -30°C; ISO 179/1eU
Charpy Impact, Notched1.7 J/cm² ISO 179/1eU

Thermal Properties
Melting Point295 °C (DAM); ISO 11357-1/-3

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.