DSM Engineering Plastics Stanyl® TE250F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, Flame Retardant (North America)


Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 46; Polymer; Thermoplastic

Key Words: Polyamide 46

Material Notes:
Information provided by DSM Engineering Plastics.

Physical PropertiesMetricEnglishComments
Density1.68 g/cc0.0607 lb/in³ (DAM); ISO 1183

Mechanical Properties
Tensile Strength at Break125 MPa18100 psi ISO 527-1/-2
Elongation at Break3.5 %3.5 % ISO 527-1/-2
Tensile Modulus8 GPa1160 ksi ISO 527-1/-2
Charpy Impact Unnotched6 J/cm²28.6 ft-lb/in² ISO 179/1eU
Charpy Impact, Notched, Low Temp0.9 J/cm²4.28 ft-lb/in² at -30°C; ISO 179/1eU
Charpy Impact, Unnotched Low Temp5 J/cm²23.8 ft-lb/in² at -30°C; ISO 179/1eU
Charpy Impact, Notched1.1 J/cm²5.24 ft-lb/in² ISO 179/1eU

Electrical Properties
Volume Resistivity1e+008 ohm-cm1e+008 ohm-cm IEC 60093
Dielectric Strength20 kV/mm508 kV/in IEC 60243-1
Comparative Tracking Index325 V325 V IEC 60112

Thermal Properties
Melting Point295 °C563 °F (DAM); ISO 11357-1/-3

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.