Physical PropertiesMetricEnglishComments
Density1.29 g/cc0.0466 lb/in³ (DAM); ISO 1183

Mechanical Properties
Tensile Strength at Break70 MPa10200 psi ISO 527-1/-2
Elongation at Break8 %8 % ISO 527-1/-2
Tensile Modulus2.8 GPa406 ksi ISO 527-1/-2
Charpy Impact, Notched1.3 J/cm²6.19 ft-lb/in² ISO 179/1eU

Electrical Properties
Volume Resistivity1e+007 ohm-cm1e+007 ohm-cm IEC 60093
Comparative Tracking Index400 V400 V IEC 60112

Thermal Properties
Melting Point295 °C563 °F (DAM); ISO 11357-1/-3

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.