DSM Engineering Plastics Stanyl® TW200F6 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized (North America)


Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 46; Polymer; Thermoplastic

Key Words: Polyamide 46

Material Notes:
Information provided by DSM Engineering Plastics.

Physical PropertiesOriginal ValueComments
Density1.41 g/cc ISO 1183
Moisture Absorption at Equilibrium2.6 % 50% RH / 23°C; Similar to ISO 62

Mechanical Properties
Tensile Strength at Break210 MPa ISO 527-1/-2
Elongation at Break4 % ISO 527-1/-2
Tensile Modulus10 GPa ISO 527-1/-2
Charpy Impact Unnotched8 J/cm² ISO 179/1eU
Charpy Impact, Notched, Low Temp1 J/cm² at -30°C; ISO 179/1eU
Charpy Impact, Unnotched Low Temp7 J/cm² at -30°C; ISO 179/1eU
Charpy Impact, Notched1.2 J/cm² ISO 179/1eU

Electrical Properties
Volume Resistivity1e+012 ohm-cm IEC 60093
Dielectric Strength30 kV/mm IEC 60243-1
Comparative Tracking Index300 V IEC 60112

Thermal Properties
CTE, linear 20°C20 µm/m-°C parallel to flow; ISO 11359-1/-2
CTE, linear 20°C Transverse to Flow80 µm/m-°C ISO 11359-1/-2
Melting Point295 °C ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi)290 °C ISO 75-1/-2

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.