DSM Engineering Plastics Stanyl® TW275F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, Molydisulfide Lubricated (North America)


Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 46; Polymer; Thermoplastic

Key Words: Polyamide 46

Material Notes:
Information provided by DSM Engineering Plastics.

Physical PropertiesMetricEnglishComments
Density1.43 g/cc0.0517 lb/in³ (DAM); ISO 1183

Mechanical Properties
Tensile Strength at Break115 MPa16700 psi ISO 527-1/-2
Elongation at Break7 %7 % ISO 527-1/-2
Tensile Modulus6 GPa870 ksi ISO 527-1/-2
Flexural Modulus6 GPa870 ksi ISO 178
Izod Impact, Notched (ISO)15 kJ/m²7.14 ft-lb/in² ISO 180/1A
Izod Impact, Notched, Low Temp (ISO)8 kJ/m²3.81 ft-lb/in² at -40°C; ISO 180/1A

Thermal Properties
Melting Point295 °C563 °F (DAM); ISO 11357-1/-3

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.