MatWeb, The Online Materials Database
DSM Engineering Plastics Stanyl® TW363 (COND) Nylon 46 Heat Stabilized, Impact Modified (North America)
Subcategory: Nylon; Nylon 46; Polymer; Thermoplastic
Key Words: Polyamide 46
Material Notes: Information provided by DSM Engineering Plastics.
| Physical Properties | Metric | English | Comments |
|
| Density | 1.1 g/cc | 0.0397 lb/in³ | (DAM); ISO 1183 |
Mechanical Properties |
|
| Tensile Strength, Yield | 45 MPa | 6530 psi | ISO 527-1/-2 |
| Elongation at Yield | Min 50 % | Min 50 % | Nominal Strain at Yield; ISO 527-1/-2 |
| Tensile Modulus | 0.6 GPa | 87 ksi | ISO 527-1/-2 |
| Charpy Impact Unnotched | NB | NB | ISO 179/1eU |
| Charpy Impact, Notched, Low Temp | 3 J/cm² | 14.3 ft-lb/in² | at -30°C; ISO 179/1eU |
| Charpy Impact, Unnotched Low Temp | NB | NB | at -30°C; ISO 179/1eU |
| Charpy Impact, Notched | 12.5 J/cm² | 59.5 ft-lb/in² | ISO 179/1eU |
Electrical Properties |
|
| Volume Resistivity | 1e+007 ohm-cm | 1e+007 ohm-cm | IEC 60093 |
| Dielectric Strength | 15 kV/mm | 381 kV/in | IEC 60243-1 |
| Comparative Tracking Index | 475 V | 475 V | IEC 60112 |
Thermal Properties |
|
| Melting Point | 295 °C | 563 °F | (DAM); ISO 11357-1/-3 |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |