MatWeb, The Online Materials Database
DSM Arnitel® EM402-L Injection Molding; Coating Grade Copolyester Elastomer (North America)
Subcategory: Elastomer, TPE; Polyester TPE; Polymer; Thermoplastic
Material Notes: Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers. Arnitel does not require vulcanization. This leads to substantial reductions in part cost. Arnitel can be used over a wide range of temperatures. Arnitel has exceptional fatigue, creep resistance and resistance to oils, greases and many other chemicals. Characteristics of Arnitel: - Excellent strength over a wide range of temperatures
- Excellent dynamic properties e.g. creep and fatigue
- High heat resistance
- Exceptional resistance to oils and greases
- Good chemical resistance
- High degree of versatility in processing
- Easy coloring using masterbatches
- Surface quality from high gloss to textured
- Excellent heat resistance (long term 165°C)
- Good electrical insulation properties
- Low moisture absorption, excellent dimensional stability
- Easy flow, fast cooling times
Typical Applications: - Automotive: Arnitel® is extensively used in the automotive industry for applications requiring exceptional fatigue resistance and resistance to oil and greases. Examples are: Rack and Pinion Bellows, Constant Velocity Joint Boots (CVJ Boots), Air brake tubings.
- Arnitel in the Electronic and Consumer Goods Industry: Arnitel® finds enormous potential and is also widely used in the consumer electronics by some of the world's best companies. Arnitel® is the best choice for low noise gears where their exceptional processability without any defects such as flash, makes it the material solution of choice. Arnitel® is also used in highly demanding applications such as in mobile phone antennas.
Arnitel® has exceptional flexibility and can perform or even outperform functions that normally require conventional rubbers. Available in a wide range of hardnesses, Arnitel can replace metals, thermoplastics, leather and rubber, often with a reduction in finished part costs. Information provided by DSM.
| Physical Properties | Metric | English | Comments |
|
| Density | 1.1 g/cc | 0.0397 lb/in³ | ISO 1183 |
| Water Absorption | 0.7 % | 0.7 % | Sim. to ISO 62 |
| Moisture Absorption at Equilibrium | 0.3 % | 0.3 % | Humidity Absorption; Sim. to ISO 62 |
| Melt Flow | 33 g/10 min | 33 g/10 min | Calculated from Volume Flow Rate of 30 cm3/10 min, 2.16 kg, 230°C; ISO 1133 |
Mechanical Properties |
|
| Hardness, Shore D | 36 | 36 | 3 s; ISO 868 |
| Tensile Strength at Break | 25 MPa | 3630 psi | ISO 527-1/-2 |
| Tensile Strength, Yield | 2.4 MPa | 348 psi | Stress at 5% Strain; ISO 527-1/-2 |
| Tensile Strength, Yield | 3.9 MPa | 566 psi | Stress at 10% Strain; ISO 527-1/-2 |
| Tensile Strength, Yield | 6.9 MPa | 1000 psi | Stress at 50% Strain; ISO 527-1/-2 |
| Tensile Strength, Yield | 7.5 MPa | 1090 psi | Stress at 100% Strain; ISO 527-1/-2 |
| Elongation at Break | Min 300 % | Min 300 % | ISO 527-1/-2 |
| Elongation at Yield | 74 % | 74 % | ISO 527-1/-2 |
| Tensile Modulus | 0.05 GPa | 7.25 ksi | ISO 527-1/-2 |
| Izod Impact, Notched (ISO) | NB | NB | 23°C; ISO 180/1A |
| Izod Impact, Unnotched Low Temp (ISO) | NB | NB | -40°C; ISO 180/1A |
| Izod Impact, Unnotched Low Temp (ISO) | NB | NB | -20°C; ISO 180/1A |
| Charpy Impact, Notched, Low Temp | NB | NB | -30°C; ISO 179/1eA |
| Charpy Impact, Notched | NB | NB | 23°C; ISO 179/1eA |
| Tensile Impact Strength | 218 kJ/m² | 104 ft-lb/in² | 23°C; ISO 8256/1 |
| Graves Tear Strength | 60 kN/m | 342 pli | without nick; ISO 34 |
Electrical Properties |
|
| Volume Resistivity | 5e+014 ohm-cm | 5e+014 ohm-cm | IEC 60093 |
| Surface Resistance | Min 1e+015 ohm | Min 1e+015 ohm | IEC 60093 |
| Dielectric Constant | 4 | 4 | 1 MHz; IEC 60250 |
| Dielectric Constant, Low Frequency | 4.1 | 4.1 | 100Hz; IEC 60250 |
| Dielectric Strength | 20 kV/mm | 508 kV/in | IEC 60243-1 |
| Dissipation Factor | 0.017 | 0.017 | 1 MHz; IEC 60250 |
| Dissipation Factor, Low Frequency | 0.001 | 0.001 | 100 Hz; IEC 60250 |
| Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
Thermal Properties |
|
| CTE, linear 20°C | 220 µm/m-°C | 122 µin/in-°F | Parallel; ISO 11359-1/-2 |
| CTE, linear 20°C Transverse to Flow | 220 µm/m-°C | 122 µin/in-°F | Normal; ISO 11359-1/-2 |
| Melting Point | 195 °C | 383 °F | 10°C/min; ISO 11357-1/-3 |
| Vicat Softening Point | 140 °C | 284 °F | 50°C/h 10N; ISO 306 |
| Glass Temperature | -78 °C | -108 °F | 10°C/min; ISO 11357-1/-2 |
| Flammability, UL94 | HB | HB | 1.6 mm nominal thickness; IEC 60695-11-10 |
Descriptive Properties | |
| Coating | Yes | |
| High impact or impact modified | Yes | |
| Injection Molding | Yes | |
| U.V. stabilized or stable to weather | Yes | |
| Without fillers | Yes | |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |