Product description: ArnitelŪ combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.

Arnitel does not require vulcanization. This leads to substantial reductions in part cost. Arnitel can be used over a wide range of temperatures. Arnitel has exceptional fatigue, creep resistance and resistance to oils, greases and many other chemicals.

Characteristics of Arnitel:

  • Excellent strength over a wide range of temperatures
  • Excellent dynamic properties e.g. creep and fatigue
  • High heat resistance
  • Exceptional resistance to oils and greases
  • Good chemical resistance
  • High degree of versatility in processing
  • Easy coloring using masterbatches
  • Surface quality from high gloss to textured
  • Excellent heat resistance (long term 165°C)
  • Good electrical insulation properties
  • Low moisture absorption, excellent dimensional stability
  • Easy flow, fast cooling times

Typical Applications:

  • Automotive: ArnitelŪ is extensively used in the automotive industry for applications requiring exceptional fatigue resistance and resistance to oil and greases. Examples are: Rack and Pinion Bellows, Constant Velocity Joint Boots (CVJ Boots), Air brake tubings.
  • Arnitel in the Electronic and Consumer Goods Industry: ArnitelŪ finds enormous potential and is also widely used in the consumer electronics by some of the world's best companies. ArnitelŪ is the best choice for low noise gears where their exceptional processability without any defects such as flash, makes it the material solution of choice. ArnitelŪ is also used in highly demanding applications such as in mobile phone antennas.

ArnitelŪ has exceptional flexibility and can perform or even outperform functions that normally require conventional rubbers. Available in a wide range of hardnesses, Arnitel can replace metals, thermoplastics, leather and rubber, often with a reduction in finished part costs.

Information provided by DSM.

Physical PropertiesMetricEnglishComments
Density1.26 g/cc0.0455 lb/inģ ISO 1183
Melt Flow37.8 g/10 min37.8 g/10 min Calculated from Volume Flow Rate of 30 cm3/10 min, 2.16 kg, 230°C; ISO 1133

Mechanical Properties
Hardness, Shore D6363 3 s; ISO 868
Tensile Strength at Break34.4 MPa4990 psi ISO 527-1/-2
Tensile Strength, Yield17.1 MPa2480 psi Stress at 5% Strain; ISO 527-1/-2
Tensile Strength, Yield22.9 MPa3320 psi Stress at 10% Strain; ISO 527-1/-2
Tensile Strength, Yield23.2 MPa3360 psi Stress at 100% Strain; ISO 527-1/-2
Tensile Strength, Yield23.2 MPa3360 psi Stress at 50% Strain; ISO 527-1/-2
Elongation at Break350 %350 % ISO 527-1/-2
Tensile Modulus0.57 GPa82.7 ksi ISO 527-1/-2
Izod Impact, Notched (ISO)21 kJ/mē9.99 ft-lb/inē 23°C; ISO 180/1A
Izod Impact, Unnotched Low Temp (ISO)5 kJ/mē2.38 ft-lb/inē -20°C; ISO 180/1A
Charpy Impact, Notched, Low Temp0.7 J/cmē3.33 ft-lb/inē -30°C; ISO 179/1eA
Charpy Impact, Notched2.3 J/cmē10.9 ft-lb/inē 23°C; ISO 179/1eA
Graves Tear Strength150 kN/m856 pli without nick; ISO 34

Thermal Properties
Melting Point221 °C430 °F 10°C/min; ISO 11357-1/-3
Flammability, UL94HBHB 1.6 mm nominal thickness; IEC 60695-11-10

Descriptive Properties
High impact or impact modifiedYes 
Injection MoldingYes 
Without fillersYes 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.