MatWeb, The Online Materials Database
DSM ArnitelŪ PM650 General Purpose Grade Copolyester Elastomer (North America)
Subcategory: Elastomer, TPE; Polyester TPE; Polymer; Thermoplastic
Material Notes: Product description: ArnitelŪ combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers. Arnitel does not require vulcanization. This leads to substantial reductions in part cost. Arnitel can be used over a wide range of temperatures. Arnitel has exceptional fatigue, creep resistance and resistance to oils, greases and many other chemicals. Characteristics of Arnitel: - Excellent strength over a wide range of temperatures
- Excellent dynamic properties e.g. creep and fatigue
- High heat resistance
- Exceptional resistance to oils and greases
- Good chemical resistance
- High degree of versatility in processing
- Easy coloring using masterbatches
- Surface quality from high gloss to textured
- Excellent heat resistance (long term 165°C)
- Good electrical insulation properties
- Low moisture absorption, excellent dimensional stability
- Easy flow, fast cooling times
Typical Applications: - Automotive: ArnitelŪ is extensively used in the automotive industry for applications requiring exceptional fatigue resistance and resistance to oil and greases. Examples are: Rack and Pinion Bellows, Constant Velocity Joint Boots (CVJ Boots), Air brake tubings.
- Arnitel in the Electronic and Consumer Goods Industry: ArnitelŪ finds enormous potential and is also widely used in the consumer electronics by some of the world's best companies. ArnitelŪ is the best choice for low noise gears where their exceptional processability without any defects such as flash, makes it the material solution of choice. ArnitelŪ is also used in highly demanding applications such as in mobile phone antennas.
ArnitelŪ has exceptional flexibility and can perform or even outperform functions that normally require conventional rubbers. Available in a wide range of hardnesses, Arnitel can replace metals, thermoplastics, leather and rubber, often with a reduction in finished part costs. Information provided by DSM.
Physical Properties | Metric | English | Comments |
|
Density | 1.26 g/cc | 0.0455 lb/inģ | ISO 1183 |
Melt Flow | 5.04 g/10 min | 5.04 g/10 min | Calculated from Volume Flow Rate of 4 cm3/10 min, 2.16 kg, 230°C; ISO 1133 |
Mechanical Properties |
|
Hardness, Shore D | 63 | 63 | 3 s; ISO 868 |
Tensile Strength at Break | 26.8 MPa | 3890 psi | ISO 527-1/-2 |
Tensile Strength, Yield | 16.6 MPa | 2410 psi | Stress at 5% Strain; ISO 527-1/-2 |
Tensile Strength, Yield | 22.7 MPa | 3290 psi | Stress at 10% Strain; ISO 527-1/-2 |
Tensile Strength, Yield | 25.5 MPa | 3700 psi | Stress at 100% Strain; ISO 527-1/-2 |
Tensile Strength, Yield | 25.6 MPa | 3710 psi | Stress at 50% Strain; ISO 527-1/-2 |
Elongation at Break | 175 % | 175 % | ISO 527-1/-2 |
Elongation at Yield | 26.3 % | 26.3 % | ISO 527-1/-2 |
Tensile Modulus | 0.52 GPa | 75.4 ksi | ISO 527-1/-2 |
Izod Impact, Notched (ISO) | 37 kJ/mē | 17.6 ft-lb/inē | 23°C; ISO 180/1A |
Izod Impact, Notched (ISO) | 8 kJ/mē | 3.81 ft-lb/inē | -20°C; ISO 180/4A |
Charpy Impact, Notched, Low Temp | 1.1 J/cmē | 5.24 ft-lb/inē | -30°C; ISO 179/1eA |
Charpy Impact, Notched | 3.7 J/cmē | 17.6 ft-lb/inē | 23°C; ISO 179/1eA |
Thermal Properties |
|
Melting Point | 221 °C | 430 °F | 10°C/min; ISO 11357-1/-3 |
Flammability, UL94 | HB | HB | 1.6 mm nominal thickness; IEC 60695-11-10 |
Descriptive Properties | |
Film Extrusion | Yes | |
High impact or impact modified | Yes | |
Other Extrusion | Yes | |
Profile Extrusion | Yes | |
Sheet Extrusion | Yes | |
Without fillers | Yes | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|