MatWeb, The Online Materials Database

DSM Arnitel® UM551-V 55 Shore D, Flame Retardant (halogen-, phosphorous-free) Copolyester Elastomer (North America)


Subcategory: Elastomer, TPE; Polyester TPE; Polymer; Thermoplastic

Material Notes:
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.

Arnitel does not require vulcanization. This leads to substantial reductions in part cost. Arnitel can be used over a wide range of temperatures. Arnitel has exceptional fatigue, creep resistance and resistance to oils, greases and many other chemicals.

Characteristics of Arnitel:

  • Excellent strength over a wide range of temperatures
  • Excellent dynamic properties e.g. creep and fatigue
  • High heat resistance
  • Exceptional resistance to oils and greases
  • Good chemical resistance
  • High degree of versatility in processing
  • Easy coloring using masterbatches
  • Surface quality from high gloss to textured
  • Excellent heat resistance (long term 165°C)
  • Good electrical insulation properties
  • Low moisture absorption, excellent dimensional stability
  • Easy flow, fast cooling times

Typical Applications:

  • Automotive: Arnitel® is extensively used in the automotive industry for applications requiring exceptional fatigue resistance and resistance to oil and greases. Examples are: Rack and Pinion Bellows, Constant Velocity Joint Boots (CVJ Boots), Air brake tubings.
  • Arnitel in the Electronic and Consumer Goods Industry: Arnitel® finds enormous potential and is also widely used in the consumer electronics by some of the world's best companies. Arnitel® is the best choice for low noise gears where their exceptional processability without any defects such as flash, makes it the material solution of choice. Arnitel® is also used in highly demanding applications such as in mobile phone antennas.

Arnitel® has exceptional flexibility and can perform or even outperform functions that normally require conventional rubbers. Available in a wide range of hardnesses, Arnitel can replace metals, thermoplastics, leather and rubber, often with a reduction in finished part costs.

Information provided by DSM.

Physical PropertiesOriginal ValueComments
Density1.28 g/cc ISO 1183
Water Absorption0.6 % Sim. to ISO 62
Moisture Absorption at Equilibrium0.25 % Humidity Absorption; Sim. to ISO 62

Mechanical Properties
Tensile Strength, Yield16.5 MPa ISO 527-1/-2
Elongation at BreakMin 50 % ISO 527-1/-2
Elongation at Yield20 % ISO 527-1/-2
Tensile Modulus0.25 GPa ISO 527-1/-2
Charpy Impact, NotchedNB 23°C; ISO 179/1eA

Electrical Properties
Comparative Tracking Index600 V IEC 60112

Thermal Properties
Melting Point200 °C 10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi)85 °C ISO 75-1/-2
Vicat Softening Point90 °C 50°C/h 50N; ISO 306

Descriptive Properties
Film ExtrusionYes 
Flame retardantYes 
Flame retarding agentYes 
Heat stabilized or stable to heatYes 
High impact or impact modifiedYes 
Injection MoldingYes 
Light stabilized or stable to lightYes 
U.V. stabilized or stable to weatherYes 
Without fillersYes 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.