MatWeb, The Online Materials Database

DSM Stanyl® TS250F6D Nylon 46-30% Glass Reinforced (Asian Grade) (Cond)


Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 46; Polymer; Thermoplastic

Material Notes:
Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:

  • Highest mechanical properties at high temperatures
  • Excellent resistance to wear and low friction
  • Outstanding flow for easy processing and exceptional design freedom
  • Stanyl High Flowgrades that match the best flowing LCPs while maintaining a high level of mechanical properties

Key Applications:

  • Automotive: Powertrain components, Charge-air coolers, EPS and ETC gears, Motor Sensors, Auto connectors, Chain tensioners
  • E&E: Connectors, Microswitches, Bobbins, Memory modules, Motor components, Industrial, Specialty films and fibers, Consumer appliances

    Information provided by DSM.

    Physical PropertiesMetricEnglishComments
    Density1.68 g/cc0.0607 lb/in³ DAM; ISO 1183

    Mechanical Properties
    Tensile Strength at Break125 MPa18100 psi ISO 527-1/-2
    Elongation at Break3.5 %3.5 % ISO 527-1/-2
    Tensile Modulus8 GPa1160 ksi ISO 527-1/-2
    Charpy Impact, Notched, Low Temp0.9 J/cm²4.28 ft-lb/in² At -30°C; ISO 179/1eA
    Charpy Impact, Notched1.1 J/cm²5.24 ft-lb/in² At 23°C; ISO 179/1eA

    Thermal Properties
    Melting Point295 °C563 °F 10°C/min (DAM); ISO 11357-1/-3

  •  


    Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.