MatWeb, The Online Materials Database
DSM Stanyl® TW241F6 Nylon 46-30% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Dry)
Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 46; Polymer; Thermoplastic
Material Notes: Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:- Highest mechanical properties at high temperatures
- Excellent resistance to wear and low friction
- Outstanding flow for easy processing and exceptional design freedom
- Stanyl High Flowgrades that match the best flowing LCPs while maintaining a high level of mechanical properties
Key Applications: Automotive: Powertrain components, Charge-air coolers, EPS and ETC gears, Motor Sensors, Auto connectors, Chain tensionersE&E: Connectors, Microswitches, Bobbins, Memory modules, Motor components, Industrial, Specialty films and fibers, Consumer appliancesInformation provided by DSM.
| Physical Properties | Original Value | Comments |
|
| Density | 1.41 g/cc | ISO 1183 |
| Linear Mold Shrinkage | 0.005 cm/cm | Parallel; ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | Normal; ISO 194-4 |
Mechanical Properties |
|
| Tensile Strength at Break | 210 MPa | ISO 527-1/-2 |
| Elongation at Break | 4 % | ISO 527-1/-2 |
| Tensile Modulus | 10 GPa | ISO 527-1/-2 |
| Charpy Impact Unnotched | 8 J/cm² | At 23°C; ISO 179/1eA |
| Charpy Impact, Notched, Low Temp | 1 J/cm² | At -30°C; ISO 179/1eA |
| Charpy Impact, Unnotched Low Temp | 7 J/cm² | At -30°C; ISO 179/1eA |
| Charpy Impact, Notched | 1.2 J/cm² | At 23°C; ISO 179/1eA |
Thermal Properties |
|
| CTE, linear 20°C | 20 µm/m-°C | ISO 11359-1/-2 |
| CTE, linear 20°C Transverse to Flow | 80 µm/m-°C | ISO 11359-1/-2 |
| Melting Point | 295 °C | 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 1.8 MPa (264 psi) | 290 °C | ISO 75-1/-2 |
| Flammability, UL94 | HB | 0.75 mm; IEC 60695-11-10 |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |