MatWeb, The Online Materials Database

DuPont Zytel® 350PHS2 NC010 Nylon 612


Subcategory: Nylon; Nylon 612; Polymer; Thermoplastic

Material Notes:
Zytel® 350PHS2 NC010 is a flexible, tough, low moisture absorption polyamide 612 resin for extrusion applications; e.g. fuel lines, hose liners, and tubing requiring chemical resistance and flexibility.

Physical PropertiesOriginal ValueComments
Density1.02 g/cc DAM; ISO 1183
Specific Gravity1.03 g/cc DAM; ASTM D 792
Water Absorption0.28 % Immersion 24h; 23°C; DAM; ASTM D 570
Linear Mold Shrinkage0.022 cm/cm Flow 3.2mm (0.125in)
Linear Mold Shrinkage, Transverse0.014 cm/cm 3.2mm (0.125in)

Mechanical Properties
Hardness, Rockwell R87 DAM; ASTM D 785
Tensile Strength, Ultimate37.1 MPa 50%RH; ASTM D 638
Tensile Strength, Ultimate41 MPa DAM; ASTM D 638
Tensile Strength, Yield28 MPa DAM; ISO 527
Elongation at BreakMin 50 % DAM; Nominal; ISO 527
Elongation at Break200 % DAM; Nominal; ISO 527
Elongation at Break250 % ISO 527
Elongation at Break304 % 50%RH; ASTM D 638
Elongation at Break329 % DAM; ASTM D 638
Elongation at Yield35 % ISO 527
Tensile Modulus0.8 GPa DAM; ISO 527
Flexural Modulus0.524 GPa 50%RH; ASTM D 790
Flexural Modulus0.67 GPa DAM; ISO 178
Flexural Modulus0.828 GPa DAM; ASTM D 790
Flexural Strength18 MPa 50%RH; ASTM D 790
Flexural Strength29 MPa DAM; ASTM D 790
Izod Impact, Notched (ISO)60 kJ/m² DAM; ISO 180/1A
Izod Impact, Notched, Low Temp (ISO)12 kJ/m² -40°C; DAM; ISO 180/1A
Charpy Impact, Notched7 J/cm² DAM; ISO 179/1eA
Izod Impact, Notched135.6 J/m -40°C; DAM; ASTM D 256
Izod Impact, Notched829.4 J/m DAM; ASTM D 256

Thermal Properties
Melting Point214 °C DAM; ASTM D 3418
Melting Point215 °C 10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi)120 °C DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi)43 °C DAM; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)45 °C DAM; ISO 75-1/-2

Processing Properties
Melt Temperature230 - 290 °C 
Melt Temperature250 °C Optimum
Mold Temperature50 - 90 °C 
Mold Temperature70 °C Optimum
Drying Temperature80 °C 
Dry Time2 - 4 hour Dehumidified Dryer
Moisture ContentMax 0.05 % 

Descriptive Properties
AppearanceNatural Color 
DryingRecommended If moisture content of resin exceeds recommended level
DuPont Product CategoryToughened Resins 
DuPont Product CategoryExtrusion Resins 
DuPont Product CategoryUnreinforced Resins 
FormPellets 
Part Marking Code>PA612-HIP< ISO 11469
RegionAmericas 
RegionAsia/Pacific 
RegionEurope 
Resin IdentificationPA612-HIP ISO 1043

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.