SABIC Innovative Plastics CYCOLOY C1200HF ABS + Polycarbonate (North America)


Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.

Physical PropertiesMetricEnglishComments
Density1.15 g/cc0.0415 lb/in³ ASTM D 792
Linear Mold Shrinkage0.005 - 0.007 cm/cm0.005 - 0.007 in/in Flow, 0.125 inch; ASTM D 955
Melt Flow19 g/10 min19 g/10 min 260C/5.0 kgf; ASTM D 1238

Mechanical Properties
Tensile Strength @ Yield57.2 MPa8300 psi Type I, 2.0 in/min; ASTM D 638
Elongation at Break150 %150 % Type I, 2.0 in/min; ASTM D 638
Elongation at Yield5 %5 % Type I, 2.0 in/min; ASTM D 638
Tensile Modulus2.28 GPa330 ksi 2.0 in/min; ASTM D 638
Flexural Modulus2.34 GPa340 ksi 0.05 in/min, 2" span; ASTM D 790
Flexural Yield Strength88.3 MPa12800 psi 0.05 in/min, 2" span; ASTM D 790
Izod Impact, Notched, Low Temp4.81 J/cm9 ft-lb/in at -22F; ASTM D 256
Gardner Impact @ 23°C54.2 J40 ft-lb Instrumented Impact Total Energy, 73°F; ASTM D 3763
Gardner Impact @ 23°C54.2 J40 ft-lb Instrumented Impact Total Energy, -22F; ASTM D 3763
Izod Impact, Notched5.87 J/cm11 ft-lb/in 73F; ASTM D 256

Electrical Properties
Comparative Tracking Index250 - 400 V250 - 400 V (+/- 0.125 inch); PLC Code 2; UL 746A
Hot Wire Ignition, HWI15 - 30 sec15 - 30 sec (+/- 0.125 inch); PLC Code 3; UL 746A
High Amp Arc Ignition, HAI60 - 120 arcs60 - 120 arcs Surface (+/- 0.125 inch); PLC Code 1; UL 746A

Thermal Properties
CTE, linear 68°F72 µm/m-°C40 µin/in-°F Flow, -40F to 100F; ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi)129 °C265 °F 0.125 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)113 °C235 °F 0.125 inch, unannealed; ASTM D 648
Vicat Softening Point130 °C266 °F B/50; ISO 306
UL RTI, Electrical105 °C221 °F UL 746B
UL RTI, Mechanical with Impact80 °C176 °F UL 746B
UL RTI, Mechanical without Impact105 °C221 °F UL 746B
Flammability, UL94HBHB 0.047 in.

Descriptive Properties
CSA File No.LS88480 
UL File Number, GLOBALE161759 
UL File Number, USAE121562 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.