| Physical Properties | Metric | English | Comments |
|
| Density | 1.12 g/cc | 0.0405 lb/in³ | ASTM D 792 |
| Water Absorption | 0.1 % | 0.1 % | 24 hours @ 73F; ASTM D 570 |
| Water Absorption at Saturation | 0.4 % | 0.4 % | Equilibrium, 73F; ASTM D 570 |
| Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | 0.005 - 0.007 in/in | Flow, 0.125 inch; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.005 - 0.007 cm/cm | 0.005 - 0.007 in/in | 0.125 inch; ASTM D 955 |
| Melt Flow | 7 g/10 min | 7 g/10 min | 230C/3.8 kgf (I); ASTM D 1238 |
Mechanical Properties |
|
| Tensile Strength @ Yield | 57.9 MPa | 8400 psi | Type I, 2.0 in/min; ASTM D 638 |
| Elongation at Break | 80 % | 80 % | Type I, 2.0 in/min; ASTM D 638 |
| Elongation at Yield | 5 % | 5 % | Type I, 2.0 in/min; ASTM D 638 |
| Tensile Modulus | 2.48 GPa | 360 ksi | 2.0 in/min; ASTM D 638 |
| Flexural Modulus | 2.48 GPa | 360 ksi | 0.05 in/min, 2" span; ASTM D 790 |
| Flexural Yield Strength | 91 MPa | 13200 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Izod Impact, Notched, Low Temp | 1.07 J/cm | 2 ft-lb/in | at -22F; ASTM D 256 |
| Gardner Impact @ 23°C | 40.7 J | 30 ft-lb | Instrumented Impact Total Energy, -22F; ASTM D 3763 |
| Gardner Impact @ 23°C | 54.2 J | 40 ft-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
| Izod Impact, Notched | 5.34 J/cm | 10 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten (+/- 0.125 inch); PLC Code 5; ASTM D 495 |
| Comparative Tracking Index | 400 - 600 V | 400 - 600 V | (+/- 0.125 inch); PLC Code 1; UL 746A |
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | (+/- 0.125 inch); PLC Code 3; UL 746A |
| High Amp Arc Ignition, HAI | Min 120 arcs | Min 120 arcs | Surface (+/- 0.125 inch); PLC Code 0; UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80 mm/min | 1 - 3.15 in/min | (+/- 0.125 inch); PLC Code 2; UL 746A |
Thermal Properties |
|
| CTE, linear 68°F | 72 µm/m-°C | 40 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
| Thermal Conductivity | 0.2 W/m-K | 1.39 BTU-in/hr-ft²-°F | ASTM C 177 |
| Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 240 °F | 0.125 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 98.9 °C | 210 °F | 0.125 inch, unannealed; ASTM D 648 |
| UL RTI, Electrical | 60 °C | 140 °F | UL 746B |
| UL RTI, Mechanical with Impact | 60 °C | 140 °F | UL 746B |
| UL RTI, Mechanical without Impact | 60 °C | 140 °F | UL 746B |
| Flammability, UL94 | HB | HB | 0.059 in. |
Descriptive Properties |
|
| CSA File No. | LS88480 | |
| UL File Number, USA | E121562 | |