MatWeb, The Online Materials Database
SABIC Innovative Plastics CYCOLOY C2801 ABS + Polycarbonate (North America)
Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
| Physical Properties | Original Value | Comments |
|
| Density | 1.22 g/cc | ASTM D 792 |
| Linear Mold Shrinkage | 0.004 - 0.005 cm/cm | Flow, 0.125 inch; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.003 - 0.005 cm/cm | 0.125 inch; ASTM D 955 |
Mechanical Properties |
|
| Tensile Strength @ Break | 7500 psi | Type I, 2.0 in/min; ASTM D 638 |
| Tensile Strength @ Yield | 9000 psi | Type I, 2.0 in/min; ASTM D 638 |
| Elongation at Break | 110 % | Type I, 2.0 in/min; ASTM D 638 |
| Flexural Modulus | 395000 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Flexural Yield Strength | 13800 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Coefficient of Friction | 0.21 | Vs. Steel, Kinetic; ASTM D 1894 |
| Coefficient of Friction, Static | 0.16 | Vs. Steel; ASTM D 1894 |
| K (wear) Factor | 430 x 10-10 in³-min/ft-lb-hr | PV = 2000 psi-fpm vs Steel; GE Test |
| Izod Impact, Notched | 2.5 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
| Comparative Tracking Index | 400 - 600 V | (+/- 0.125 inch); PLC Code 1; UL 746A |
| Hot Wire Ignition, HWI | 15 - 30 sec | (+/- 0.125 inch); PLC Code 3; UL 746A |
| High Amp Arc Ignition, HAI | Min 120 arcs | Surface (+/- 0.125 inch); PLC Code 0; UL 746A |
Thermal Properties |
|
| Deflection Temperature at 1.8 MPa (264 psi) | 180 °F | 0.250 inch, unannealed; ASTM D 648 |
| UL RTI, Electrical | 60 °C | UL 746B |
| UL RTI, Mechanical with Impact | 60 °C | UL 746B |
| UL RTI, Mechanical without Impact | 60 °C | UL 746B |
| Flammability, UL94 | V-0 | 0.059 in. |
| Flammability, UL94 | 6 | 0.098 in. |
Descriptive Properties | |
| UL File Number, USA | E121562 | |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |