SABIC Innovative Plastics CYCOLOY C6200 ABS + Polycarbonate (North America)
Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
| Physical Properties | Original Value | Comments |
|
| Density | 1.18 g/cc | ASTM D 792 |
| Linear Mold Shrinkage | 0.004 - 0.006 cm/cm | Flow, 0.125 inch; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.004 - 0.006 cm/cm | 0.125 inch; ASTM D 955 |
| Melt Flow | 14.5 g/10 min | 260C/2.16 kgf; ASTM D 1238 |
| Spiral Flow | 27 in | 500F, 10 ips, .125 X 60 in |
Mechanical Properties |
|
| Tensile Strength @ Yield | 9700 psi | Type I, 2.0 in/min; ASTM D 638 |
| Elongation at Break | 50 % | Type I, 2.0 in/min; ASTM D 638 |
| Flexural Modulus | 390000 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Flexural Yield Strength | 15000 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Gardner Impact @ 23°C | 480 in-lb | Instrumented Impact Energy @ peak, -22°F; ASTM D 3763 |
| Gardner Impact @ 23°C | 540 in-lb | Instrumented Impact Energy @ peak, 73F; ASTM D 3763 |
| Izod Impact, Notched | 10 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
| Volume Resistivity | Min 1e+015 ohm-cm | IEC 60093 |
| Surface Resistivity per Square | Min 1e+015 ohm | IEC 60093 |
| Dielectric Constant | 2.7 | 1 MHz; IEC 60250 |
| Dielectric Constant | 2.8 | 50 Hz; IEC 60250 |
| Dielectric Strength | 17 kV/mm | in oil, 3.2 mm; IEC 60243-1 |
| Dielectric Strength | 25 kV/mm | in oil, 1.6 mm; IEC 60243-1 |
| Dielectric Strength | 35 kV/mm | in oil, 0.8 mm; IEC 60243-1 |
| Dissipation Factor | 0.004 | 50 Hz; IEC 60250 |
| Dissipation Factor | 0.008 | 1 MHz; IEC 60250 |
| Arc Resistance | 60 - 120 sec | Tungsten (+/- 0.125 inch); PLC Code 6; ASTM D 495 |
| Comparative Tracking Index | 250 - 400 V | (+/- 0.125 inch); PLC Code 2; UL 746A |
| Hot Wire Ignition, HWI | 30 - 60 sec | (+/- 0.125 inch); PLC Code 2; UL 746A |
| High Amp Arc Ignition, HAI | Min 120 arcs | Surface (+/- 0.125 inch); PLC Code 0; UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | 80 - 150 mm/min | (+/- 0.125 inch); PLC Code 3; UL 746A |
Thermal Properties |
|
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °F | 0.125 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °F | 0.250 inch, unannealed; ASTM D 648 |
| UL RTI, Electrical | 85 °C | UL 746B |
| UL RTI, Mechanical with Impact | 85 °C | UL 746B |
| UL RTI, Mechanical without Impact | 85 °C | UL 746B |
| Flammability, UL94 | HB | 0.028 in. |
| Flammability, UL94 | V-1 | 0.048 in. |
| Flammability, UL94 | V-0 | 0.058 in. |
| Flammability, UL94 | 6 | 0.079 in. |
| Flammability, UL94 | 7 | 0.134 in. |
Descriptive Properties | |
| CSA File No. | LS88480 | |
| UL File Number, GLOBAL | E161759 | |
| UL File Number, USA | E121562 | |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |