MatWeb, The Online Materials Database

SABIC Innovative Plastics CYCOLOY C7210A ABS + Polycarbonate (North America)


Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line.

Physical PropertiesMetricEnglishComments
Density1.22 g/cc0.0441 lb/in³ ASTM D 792
Linear Mold Shrinkage0.003 - 0.005 cm/cm0.003 - 0.005 in/in Flow, 0.125 inch; ASTM D 955
Linear Mold Shrinkage, Transverse0.004 - 0.006 cm/cm0.004 - 0.006 in/in 0.125 inch; ASTM D 955
Melt Flow16.4 g/10 min16.4 g/10 min 260C/2.16 kgf; ASTM D 1238

Mechanical Properties
Tensile Strength @ Break49 MPa7100 psi Type I, 0.2 in/min; ASTM D 638
Tensile Strength @ Yield63.4 MPa9200 psi Type I, 0.2 in/min; ASTM D 638
Elongation at Break80 %80 % Type I, 0.2 in/min; ASTM D 638
Elongation at Yield3.6 %3.6 % Type I, 0.2 in/min; ASTM D 638
Tensile Modulus3.52 GPa510 ksi 0.2 in/min; ASTM D 638
Flexural Modulus3.14 GPa456 ksi 0.05 in/min, 2" span; ASTM D 790
Flexural Strength106 MPa15400 psi 0.05 in/min, 2" span; ASTM D 790
Izod Impact, Unnotched18.7 J/cm35 ft-lb/in 73F; ASTM D 4812
Gardner Impact @ 23°C47.5 J35 ft-lb Instrumented Impact Total Energy, 73°F; ASTM D 3763
Izod Impact, Notched1.76 J/cm3.3 ft-lb/in 73F; ASTM D 256

Thermal Properties
CTE, linear 68°F59.4 µm/m-°C33 µin/in-°F Flow, -40F to 100F; ASTM E 831
CTE, linear 68°F, Transverse to Flow66.6 µm/m-°C37 µin/in-°F from -40F to 100F; ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi)92.2 °C198 °F 0.125 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)82.2 °C180 °F 0.125 inch, unannealed; ASTM D 648
Vicat Softening Point102 °C215 °F Rate B; ASTM D 1525
UL RTI, Electrical60 °C140 °F UL 746B
UL RTI, Mechanical with Impact60 °C140 °F UL 746B
UL RTI, Mechanical without Impact60 °C140 °F UL 746B
Flammability, UL94V-0V-0 0.047 in.
Flammability, UL9466 0.078 in.

Descriptive Properties
UL File Number, GLOBALE161759 
UL File Number, USAE121562 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.