MatWeb, The Online Materials Database
SABIC Innovative Plastics CYCOLOY FXC810MA ABS + Polycarbonate (North America)
Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
Physical Properties | Metric | English | Comments |
|
Density | 1.18 g/cc | 0.0426 lb/in³ | ASTM D 792 |
Linear Mold Shrinkage | 0.004 - 0.006 cm/cm | 0.004 - 0.006 in/in | Flow, 0.125 inch; ASTM D 955 |
Melt Flow | 22 g/10 min | 22 g/10 min | 260C/5.0 kgf; ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Break | 44.8 MPa | 6500 psi | Type I, 2.0 in/min; ASTM D 638 |
Tensile Strength @ Yield | 51.7 MPa | 7500 psi | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Break | 50 % | 50 % | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Yield | 5 % | 5 % | Type I, 2.0 in/min; ASTM D 638 |
Tensile Modulus | 2.48 GPa | 360 ksi | 2.0 in/min; ASTM D 638 |
Flexural Modulus | 2.41 GPa | 350 ksi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Yield Strength | 75.8 MPa | 11000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Gardner Impact @ 23°C | 40.7 J | 30 ft-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
Izod Impact, Notched | 4.27 J/cm | 8 ft-lb/in | 73F; ASTM D 256 |
Thermal Properties |
|
CTE, linear 68°F | 72 µm/m-°C | 40 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
CTE, linear 68°F, Transverse to Flow | 72 µm/m-°C | 40 µin/in-°F | from -40F to 100F; ASTM E 831 |
Deflection Temperature at 0.46 MPa (66 psi) | 131 °C | 268 °F | 0.125 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C | 235 °F | 0.125 inch, unannealed; ASTM D 648 |
Vicat Softening Point | 143 °C | 290 °F | Rate B; ASTM D 1525 |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |