SABIC Innovative Plastics CYCOLOY IP1000 ABS + Polycarbonate (North America)
Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
| Physical Properties | Original Value | Comments |
|
| Density | 1.13 g/cc | ASTM D 792 |
| Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | Flow, 0.125 inch; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.005 - 0.007 cm/cm | 0.125 inch; ASTM D 955 |
| Melt Flow | 14.5 g/10 min | 260C/5.0 kgf; ASTM D 1238 |
Mechanical Properties |
|
| Tensile Strength @ Break | 8700 psi | Type I, 2.0 in/min; ASTM D 638 |
| Tensile Strength @ Yield | 8000 psi | Type I, 2.0 in/min; ASTM D 638 |
| Elongation at Break | 150 % | Type I, 2.0 in/min; ASTM D 638 |
| Elongation at Yield | 8 % | Type I, 2.0 in/min; ASTM D 638 |
| Tensile Modulus | 310000 psi | 2.0 in/min; ASTM D 638 |
| Flexural Modulus | 328000 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Flexural Yield Strength | 12300 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Izod Impact, Notched, Low Temp | 10 ft-lb/in | at -22F; ASTM D 256 |
| Gardner Impact @ 23°C | 500 in-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
| Gardner Impact @ 23°C | 550 in-lb | Instrumented Impact Total Energy, -22F; ASTM D 3763 |
| Izod Impact, Notched | 12.5 ft-lb/in | 73F; ASTM D 256 |
Thermal Properties |
|
| CTE, linear 68°F | 44 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
| CTE, linear 68°F, Transverse to Flow | 44 µin/in-°F | from -40F to 100F; ASTM E 831 |
| Deflection Temperature at 0.46 MPa (66 psi) | 261 °F | 0.125 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 230 °F | 0.125 inch, unannealed; ASTM D 648 |
| Vicat Softening Point | 288 °F | Rate B; ASTM D 1525 |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |