Physical PropertiesOriginal ValueComments
Density1.13 g/cc ASTM D 792
Linear Mold Shrinkage0.005 - 0.007 cm/cm Flow, 0.125 inch; ASTM D 955
Melt Flow6.5 g/10 min 260C/5.0 kgf; ASTM D 1238

Mechanical Properties
Tensile Strength @ Yield8100 psi Type I, 2.0 in/min; ASTM D 638
Elongation at Break120 % Type I, 2.0 in/min; ASTM D 638
Elongation at Yield5 % Type I, 2.0 in/min; ASTM D 638
Flexural Modulus330000 psi 0.05 in/min, 2" span; ASTM D 790
Flexural Yield Strength12400 psi 0.05 in/min, 2" span; ASTM D 790
Izod Impact, Notched, Low Temp11 ft-lb/in at -22F; ASTM D 256
Gardner Impact @ 23°C360 in-lb Instrumented Impact Total Energy, -22F; ASTM D 3763
Gardner Impact @ 23°C420 in-lb Instrumented Impact Total Energy, 73°F; ASTM D 3763
Izod Impact, Notched12 ft-lb/in 73F; ASTM D 256

Thermal Properties
CTE, linear 68°F50 µin/in-°F Flow, -40F to 100F; ASTM E 831
Thermal Conductivity0.25 W/m-K ASTM C 177
Deflection Temperature at 0.46 MPa (66 psi)250 °F 0.125 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)220 °F 0.125 inch, unannealed; ASTM D 648

Optical Properties
Gloss30 % Untextured, 60 degrees; ASTM D 523

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.